MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Fomblin® M07 PFPE Lubricant  (Unverified Data**)
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: The following properties and characteristics of Fomblin® PFPE lubricants are sure to include some that are important to your application:
  • Unmatched chemical and solvent resistance
  • Excellent thermal resistance
  • Excellent electrical resistance
  • Non-reactive with metal, plastic, elastomers and rubber
  • Inert to liquid and gaseous oxygen
  • Excellent radiation hardness
  • Good viscosity index
  • Nonflammable
  • Extremely wide operating temperature range
  • Low evaporation loss
  • Excellent water washout properties
  • Good low and high temperature wear properties
  • Easily formulated into greases
  • Environmentally safe
  • Non-toxic behavior
In addition, certain grades of Fomblin® PFPE lubricants also offer special features such as:
  • Extremely high viscosity index (< 300)
  • Excellent low temperature starting torque
  • Improved evaporation characteristics
The availability of additivated Fomblin® PFPE fluids widens the range of applications for perfluorinated fluids and greases in fields demanding high anti-rust properties. These applications include lubrication of bearings, gears, turbine and liquid compressors that may be in contact with condensed water vapor. These additives also provide an opportunity to use Fomblin® PFPE as a hydraulic fluid, filling fluid and solvents where antirust prevention is one of the primary product specifications.

While Fomblin® PFPE lubricants can be used in their original form, they are often formulated into greases for specific applications in the chemical, electronic, military, nuclear, data processing and other industries in need of high performance lubrication. A few of the critical uses of Fomblin® PFPE lubricants include:

  • Tenter frames in the textile industry
  • Deep space rocket nozzle lubrication
  • Missile catapult system lubrication
  • Sintered metal bearing requiring exceptional operating life
  • Anti-lock braking systems
  • Oxygen and chlorine valves and pumping systems
  • Sealing fluid for vacuum pumps
  • Gold contact surface lubrication
  • Nuclear industry lubricants
  • Instrument lubricants
  • Lifetime sealed, maintenance-free bearings
  • Lubricants for gasoline tank floats
  • Bearings exposed to high temperatures, moisture and aggressive chemicals

Information provided by Solvay

Vendors:
Available Properties
  • Density, ASTM D4052
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Kinematic Viscosity, ASTM D445
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Molecular Weight
  • Evaporation Loss, ASTM D2595
  • Surface Tension, ASTM D1331
  • Four Ball Wear, ASTM D4172, 1200 rpm, 40 kg, Avg scar diameter
  • Pour Point, ASTM D97
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
none

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.