MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensional stability and warp resistance during injection molding. The AV-651 CF30 grade offers the highest strength, stiffness, and fatigue resistance of any AV-651-based grade. Furthermore, this resin generally retains most of the desirable ultra-performance attributes of carbon fiber reinforced PEEK. Those attributes include chemical resistance, fatigue resistance, and long term thermal oxidative stability. The excellent balance of properties of AV-651 CF30 makes this grade well suited for a broad range of applications across a number of industries. This resin can be easily melt processed by injection molding using standard equipment. The melt processing behavior of AV-651 CF30 is overall very similar to that of 30% CF reinforced PEEK. While the resin can also be extruded, the lower melt flow AV-621 CF30 grade is considered more suited for extrusion applications while offering the same property profile as AV-651 CF30.

Autoclave Sterilizable; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable

Uses: Dental Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Pump Parts; Seals; Surgical Instruments

Processing: Injection Molding; Machining; Profile Extrusion

Agency Ratings: ISO 10993

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Viscosity, ASTM D3835, Melt
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell M, ASTM D785
  • Hardness, Shore D
  • Tensile Strength, ASTM D638, 5.0 mm/min
  • Tensile Strength, Yield, ISO 527-2, Type 1A, 5 mm/min
  • Elongation at Break, ASTM D638, 5.0 mm/min
  • Elongation at Break, ISO 527-2, Type 1A, 5 mm/min
  • Tensile Modulus, ASTM D638, 5.0 mm/min
  • Tensile Modulus, ISO 527-2, 1 mm/min, Type 1A
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • CTE, linear, Parallel to Flow, ASTM E831
  • Specific Heat Capacity, ASTM C351
  • Specific Heat Capacity, ASTM C351
  • Thermal Conductivity, ASTM C177
  • Melting Point, ASTM D3418, Peak
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Glass Transition Temp, Tg, DSC
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.