MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Sika SikaBond® Construction Adhesive One part advanced polyurethane, elastomeric adhesive
Categories: Polymer; Adhesive

Material Notes: SikaBond Construction Adhesive is a one-component, gun-grade, adhesive and sealing compound of permanent elasticity. This dual-purpose material is based on a special moisture-cured polyurethane with an accelerated curing time.

Where to Use As an elastic adhesive for:

  • Paver caps, masonry veneer and Faux stone.
  • Cover plates, gaskets and coverings.
  • Acoustic ceiling tiles.
  • Floor moldings and door sills.
  • Light weight construction materials.
  • Wood, metal, or plastic window and door frames.
  • Roof tiles.
As an elastic joint sealer for:
  • Air ducts and high vacuum systems.
  • Containers, tanks, and silos.
  • Gaskets in openings in walls or floors for ducts, piling, etc.
  • Reservoirs or water retaining structures.
  • Aluminum fabrication.
  • Bolted lap joints.
Advantages:
  • Excellent adhesion on all cement-based materials, brick, ceramics, glass, metals, wood, epoxy, polyester, acrylic resin, and plastics.
  • Fast cure rate.
  • Waterproof and water immersible after cure.
  • Good weathering resistance.
  • Non-corrosive.
  • Can be painted over with water, oil, and rubber-based paints. (Preliminary tests recommended).
  • High durability.

Information provided by Sika Corporation.

Vendors:
Available Properties
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Processing Temperature, Application Temp; Condition material to 65°-75°F before using.
  • Cure Time, Final Cure
  • Shelf Life, in original unopened cartridge
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.