MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and ceramics, and is recommended for electrical and structural potting and encapsulating applications where the combination of good mechanical, thermal, electrical and room temperature cure properties are required. Fully cured TRA-CAST 3156 is a strong, tough, electrical insulator with high heat stability and a low thermal coefficient of expansion that provides successful performance over a wide temperature range. It is resistant to industrial environments that include water, weather, galvanic action, petroleum fuels, lubricants and solvents, gases and vapors, many mild acids and alkalis.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Volatile Organic Compounds (VOC) Content
  • Water Absorption, After 24 hours
  • Viscosity, Mixed (sp #7, 10 rpm)
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Compressive Strength
  • Adhesive Bond Strength, Lap shear, alum to alum, 24 hrs @ 25°C
  • Adhesive Bond Strength, Lap shear, alum to alum, 4 hrs @ 25°C + 2 hrs @ 65°C
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, Ultimate Tg
  • Cure Time, 4 hrs @ 25°C + 2 hrs @ 65°C
  • Cure Time
  • Pot Life, 25 grams
  • Pot Life, 100 grams
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.