Master Bond Polymer System MB529 is a high performance 100% solid acrylic resin based hot melt compound designed for use as a hot melt pressure sensitive adhesive. It exhibits good adhesion to a wide variety of materials including polyester, glass, aluminum, steel, fabric and paper. Master Bond MB529 provides a medium degree of cohesive strength with good resistance to creep or cold flow. MB529 is a thermoplastic acrylic resin which can be applied using a variety of hot melt coating equipment. |