MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Go Yen Chemical GY-FR-PTL141 Non-Halogen Backing Adhesive Flame Retard Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Flame retardant for textile; Long-term flame retardant ability; No volatility; Excellent heat stability; Non halogen

Advantages:

  • GY-FR-PTL141 can offer excellent flame retard effect.
  • GY-FR-PTL141 can apply on PU foaming product.
  • Compatible and ease dispersing with all kinds of resin and polymer.
  • Confer long term flame retard ability for end product.
  • Won’t generate migration.
  • Compatible with comprehensive and all kinds of plastic, polymer, resin, elastomer, adhesive, and compound.
Applications:
  • Adhesive backed flame retard additive
  • Other textile flame retard applications

Information provided by Go Yen Chemical

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.