- Black: AS-4133 L BK 324
- Natural: AS-4133 L NT
Chemical Resistant; Creep Resistant; Fast Molding Cycle; Good Dimensional Stability; Good Stiffness; High Strength; Hot Water Moldability; Low Moisture Absorption; Lubricated
Uses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Cell Phones; Electrical/Electronic Applications; General Purpose; Housings; Industrial Applications; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts
Processing: Water-Heated Mold Injection Molding
Automotive Specifications: ASTM D6779 PA105G35
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Property data reported in the 'Dry' condition unless noted otherwise.