MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Aptek 2210A/B Electrically conductive urethane adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Electrically conductive urethane adhesive, silver-filled, flexible low modulus, low outgassing
APTEK 2210-A/B is a two component, silver-filled, urethane adhesive designed for application where flexibility and electrically conductivity are required. APTEK 2210-A/B is a 100% solid adhesive displaying excellent adhesion to plastic metal substrates.

Non-TDI based for safety; Very flexible/low modulus to absorb stress buildup during thermal cycling; Excellent adhesion to ceramic and various substrates; Low Tg(<-60ÂșC) for excellent low temperature performance

APTEK 2210A is a silver filled polyol resin. APTEK 2210B is an organic isocyanate.

Information provided by Aptek Laboratories, Inc.

Vendors:
Available Properties
  • Density, B Component; ASTM D1475
  • Density, ASTM D1475
  • Density, A Component; ASTM D1475
  • Viscosity, B Component; ASTM D1824
  • Outgassing - Total Mass Loss, Cured property; at 10E-6 torr; ASTM E595
  • Collected Volatile Condensable Material, Cured property; at 10E-6 torr; ASTM E595
  • Volume Resistivity, Cured property; ASTM D257
  • Thermal Conductivity, COLORA
  • Flash Point, A Component; ASTM D92
  • Flash Point, B Component; ASTM D92
  • Processing Temperature, Cure 4 hrs
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.