MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
BASF 3D Ultrafuse® SEBS Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Components: Styrene-Ethylene-Butadiene-Styrene (SEBS) based filament for Fused Filament Fabrication.

Product Description: Ultrafuse® TPS 90A is an elastomer based on the raw material SEBS. The combination of durable and flexible building blocks leads to a very versatile material. Compared to other flexible 3D printing materials it shows more rubber-like soft touch haptics and better non-slip properties. Furthermore, the material shows a reduced moisture uptake, which allows for printing without pre-drying. Parts printed with Ultrafuse® TPS 90A show almost no visible layers or warpage, which makes it an excellent material choice for end-use parts. Producing multi-material parts is possible by printing it together with PP.

Information provided by BASF

Vendors:
Available Properties
  • Density, ISO 1183-1, Printed Part
  • Melt Flow, ISO 1133
  • Storage Temperature
  • Hardness, Shore A, ISO 7619-1
  • Hardness, Shore D, ISO 7619-1
  • Tensile Strength at Break, ISO 527, ZX: Upright
  • Tensile Strength at Break, ISO 527, XY: Flat
  • Tensile Stress, ISO 527, XY: Flat
  • Tensile Stress, ISO 527, XY: Flat
  • Tensile Stress, ISO 527, XY: Flat
  • Elongation at Break, ISO 527, ZX: Upright
  • Elongation at Break, ISO 527, XY: Flat
  • Modulus of Elasticity, ISO 527, Young's, ZX: Upright
  • Modulus of Elasticity, ISO 527, Young's, XY: Flat
  • Charpy Impact Unnotched, ISO 179-2, XY: Flat
  • Charpy Impact Unnotched, ISO 179-2, XZ: On its edge
  • Charpy Impact Unnotched, ISO 179-2, ZX: Upright
  • Charpy Impact, Notched, ISO 179-2, ZX: Upright
  • Charpy Impact, Notched, ISO 179-2, XY: Flat
  • Charpy Impact, Notched, ISO 179-2, XZ: On its edge
  • Tensile Impact Strength, ISO 8256-1, ZX: Upright
  • Tensile Impact Strength, ISO 8256-1, XY: Flat
  • Tensile Impact Strength, ISO 8256-1, XZ: On its edge
  • Tear Strength, ISO 34-1, ZX: Upright
  • Tear Strength, ISO 34-1, XZ: On its edge
  • Tear Strength, ISO 34-1, XY: Flat
  • Abrasion, ISO 4649, mm3
  • Compression Set, ISO 815-1
  • Compression Set, ISO 815-1
  • Melting Point, ISO 11357-3
  • Glass Transition Temp, Tg, ISO 11357-2
  • Processing Temperature, Bed, Bed Material: PEI, PI or glue
  • Nozzle Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.