MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Eastman Eastman Advantis™ 515-2 40A adhesion promoter
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eastman Advantis™ 515-2 40A adhesion promoter (40% in Aromatic 100) is a liquid at room temperature. If the solution gels due to storage at low temperatures, it can be re-liquified by warming to 38°C with agitation. Solutions of Eastman Advantis 515-2 40A adhesion promoter (as supplied) can easily be reduced with xylene, toluene, selected ketones, and ester solvents. Advantis 515-2 40A has good heat resistance and is compatible with a variety of resins. It combines with the resins to give clear solutions and deposit clear films. Advantis™ 515- 2 40A also has excellent adhesion to polypropylene and good-to-excellent adhesion to many other substrates. Advantis 515-2 40A not only adheres to a variety of substrates, but when added to coatings and inks it improves their adhesion to these substrates.

Applications

  • Auto omen
  • Commercial printing inks
  • General industrial coatings
  • Graphic arts
  • Protective coatings

Information provided by Eastman.

Vendors:
Available Properties
  • Density
  • Density, Solid CPO
  • Flash Point, Tag Closed Cup
  • Gardner Color Number
  • Chlorine, Cl
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.