MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Material Notes: Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel

Vanadis 4 Extra is characterized by:

  • Very good ductility
  • High abrasive-adhesive wear resistance
  • High compressive strength
  • Good dimensional stability during heat treatment and in service
  • Very good through hardening properties
  • Good temper back resistance
  • Good machinability and grindability

Applications:Uddeholm Vanadis 4 Extra is especially suitable for applications where adhesive wear and/or chipping are the dominating failure mechanisms, i.e.with soft/adherent materials such as austenitic stainless steel, mild steel, copper, aluminium, etc.as work material; with thicker work material and high strength work materials. Uddeholm Vanadis 4 Extra is however also very suitable for blanking and forming of Ultra High Strength Steel Sheet, these materials place high demands on the tool steel regarding abrasive wear resistance and ductility.

Vendors:
Available Properties
  • Density, hardened to 60 HRC
  • Hardness, Brinell, Soft annealed
  • Modulus of Elasticity, (hardened to 60 HRC)
  • Modulus of Elasticity, hardened to 60 HRC
  • Modulus of Elasticity, hardened to 60 HRC
  • Impact Test, HRC 65, unnotched
  • Impact Test, HRC 63, unnotched
  • Impact Test, HRC 61, unnotched
  • Impact Test, HRC 59, unnotched
  • Impact Test, HRC 57, unnotched
  • Impact Test, HRC 55, unnotched
  • CTE, linear, hardened to 60 HRC
  • CTE, linear, hardened to 60 HRC
  • Specific Heat Capacity, hardened to 60 HRC
  • Thermal Conductivity, hardened to 60 HRC
  • Thermal Conductivity, hardened to 60 HRC
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.