  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zircar Zirconia ZR-RIG Zirconia Rigidizer
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zircar Zirconia Rigidizer Type ZR-RIG is formulated for the surface hardening of all Zircar zirconia fiber products and for use in the fabrication of zirconia composites from Zircar zirconia textiles. Such composites are comprised of a matrix of zirconia fibers reinforced with sub-micron zirconia particles. Type ZR-RIG has the same fired composition as Zircar zirconia fibers and forms a fully stabilized zirconia body upon curing.

ZR- RIG contains sub-micron particles of yttria-stabilized zirconia suspended in a zirconium acetate aqueous solution. The water based rigidizer, as supplied, has the consistency of a light house paint. Should the rigidizer become too thick during use for complete penetration into the surface of the zirconia fiber product, the rigidizer can be thinned by small additions of de-ionized or distilled water.

Features:

  • High Purity
  • High Temperature Stability to 2200°C
  • Withstands Water and Steam after curing
  • Safe to Use – Non-Flammable
  • Available in Two Sizes; Pint or Quart
  • Available ‘Off the Shelf’

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors:
Available Properties
  • Specific Gravity
  • Solids Content
  • Melting Point
  • HfO2
  • Y2O3
  • ZrO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.