MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Permabond 798 Cyanoacrylate, Surface insensitive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND 798 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, Metals, Ceramics and elastomers are also rapidly bonded. The fast cure minimizes the occurrence of frosting and fogging. This adhesive is particularly well­suited for use on porous substrates, since it fixtures before wicking into the surface pores. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for  high speed production lines.

Features & Benefits:

  • Extremely Fast Setting
  • Rapid cure through large gaps 
  • Surface insensitive­cures rapidly on most surfaces
  • Easy to apply and dispense
  • 100% reactive, no solvents

Typical Applications:

  • Rubber Bonding
  • Model Assembly
  • Jewelry Assembly
  • Ceramics Bonding
  • Wood Bonding
  • Speaker Bonding
  • Fabric and leather bonding

Soluble In Nitroethane, Methyl Ethyl Ketone, Acetone

Information provided by Permabond.

Vendors:
Available Properties
  • Specific Gravity, Uncured
  • Viscosity, Uncured
  • Storage Temperature
  • Hardness, Shore A
  • Adhesive Bond Strength, Grit-blasted Steel, Shear
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point
  • Cure Time, Phenolic, set time
  • Cure Time, Buna N Rubber, set time
  • Cure Time, Steel, set time
  • Cure Time, full strength
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.