MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP36AO One Part, Thermally Conductive, Heat Resistant Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, High Temperature; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Available in 30 gram performs
  • High temperature resistant
  • Thermally conductive
  • Flexibilized and toughened
  • Unlimited working life at room temperature
  • Electrically insulative
Product Description: Master Bond EP36AO is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high temperature resistance. It differs greatly from other heat resistant epoxies as it has far more toughness and flexibility at elevated temperatures. Its forgiving nature at high temperatures imparts vastly superior thermal and mechanical shock resistance as well as superb thermal cycling ability when compared to more standard high temperature resistant epoxies. EP36AO bonds well to a variety of substrates including metals, composites, glass and many plastics. It has good chemical resistance to water, fuels and oils. This one component system is primarily used for potting but can also be used for bonding and sealing. The service temperature range is -100°F to +500°F. As mentioned above, EP36AO retains toughness and heat resistance up to 500°F without losing its critical properties. The hardness remains consistent (20-30 Shore D) above its Tg, and it is still able to withstand rigorous thermal cycling. EP36AO is ideal for potting and encapsulation applications where thermal conductivity, electrical isolation and the ability to withstand severe thermal cycling over a wide temperature range are needed. While EP36AO is an unconventional epoxy, it is conveniently available in 30 gram preforms as well as pints and quarts. This system is formulated at elevated temperatures and poured into cans or 30 gram cookie molds and solidifies. Since it is a solid; it must be heated in a forced air or convection oven at 170-180°F to transform it to a liquid. As a liquid, it is easy to apply as an encapsulant or an adhesive. To complete the cure, the temperature should be 350°F for 2-3 hours. EP36AO will retain its liquidity as long as the temperature does not exceed 180°F. Liquefied but uncured material can be reused by allowing EP36AO to resolidify at room temperature. Cured material cannot reliquefy; resolidified epoxy can become liquid again. This epoxy is off-white in color. A more detailed description of curing the 30 gram cookie appears in the cure section below EP36AO is truly a specialty type system that is primarily used in electronic and aerospace applications.

Product Advantages:

  • One component system
  • Superb thermal conductivity and electrical insulation properties
  • Combines flexibility and toughness with high temperature resistance
  • Ideal for potting and encapsulation
  • Unused material is easy to reprocess
  • Available in conveniently prepared 30 gram performs
  • Capable of withstanding rigorous thermal cycling and thermal shocks

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity
  • Hardness, Shore D
  • Hardness, Shore D
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, liquefy at minimum 170-180°F then
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.