MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP29LP Low Exotherm, Low Viscosity Two Component Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Room temperature curing epoxy
  • Low viscosity
  • Long working life
  • Low exotherm
  • Optically clear
  • Used in large encapsulation applications
Product Description: Master Bond EP29LP is a two part, high performance epoxy system featuring low viscosity, exceptionally low exotherm and a very long pot life. It has a convenient two to one mix ratio by weight and is formulated to cure at room temperature or faster at elevated temperatures. The working life of a 100 gram mass is greater than 10 hours and when mixing 1 pound, the working life exceeds 5 hours. The extraordinarily long open time is due to the system generating very little heat upon mixing. EP29LP has a formidable array of outstanding physical properties along with superb optical clarity and light transmission. It is a top notch electrical insulator and is ideally suited for moderate to larger castings. It offers superior resistance to a wide range of chemicals including water, acids, bases, oils and fuels. This system also features low shrinkage upon cure. Although it cures rigid, it has reasonably good impact resistance. It bonds well to a wide variety of substrates including metals, ceramics, glass, optical fibers, polyimide, graphite and many rubbers and plastics. The service temperature range is -60°F to +250°F. This system is 100% reactive and does not contain any solvents or diluents. Its long open time, low exotherm and electrical insulation profile allows it to be used in large encapsulations and for filament winding applications. It is widely used in a variety of industries including aerospace, electronic, optical, fiber-optic, specialty OEM and others.

Product Advantages:

  • Convenient, non-critical two to one mix ratio by weight
  • Very low viscosity, exceptionally long working life
  • Superior physical strength profile
  • Notable electrical insulation characteristics; ideal for larger potting and encapsulation applications
  • Exquisite optical clarity
  • Desirable adhesive for composites, optical fiber, fiber reinforced Materials
  • Exceptionally low shrinkage upon curing

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time, Optimum cure schedule: followed by a post cure at 200°F for 4-5 hours
  • Cure Time
  • Working Life, working life after mixing, 1 pound
  • Working Life, After mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.