Available Properties |
---|
- Specific Gravity, ASTM D792
- Filler Content
- Moisture Absorption, ASTM D570, 50%RH,23°C,24h
- Moisture Absorption at Equilibrium, ISO 62, Similar to, 50% RH
- Linear Mold Shrinkage, ASTM D955, Transverse
- Linear Mold Shrinkage, ASTM D955, Transverse
- Linear Mold Shrinkage, Flow, ASTM D955
- Linear Mold Shrinkage, Flow, ASTM D955
- Hardness, Rockwell M, ASTM D785
- Hardness, Rockwell R, ASTM D785
- Tensile Strength at Break, ISO 527
- Tensile Strength, ASTM D638
- Tensile Strength, ASTM D638
- Tensile Strength, ASTM D638
- Tensile Strength, ASTM D638
- Elongation at Break, ASTM D638
- Elongation at Break, ASTM D638
- Elongation at Break, ISO 527
- Elongation at Break, ASTM D638
- Elongation at Break, ASTM D638
- Tensile Modulus, ASTM D638
- Tensile Modulus, ASTM D638
- Tensile Modulus, ASTM D638
- Tensile Modulus, ISO 527
- Tensile Modulus, ASTM D638
- Flexural Strength, ASTM D790
- Flexural Strength, ASTM D790
- Flexural Strength, ASTM D790
- Flexural Strength, ASTM D790
- Flexural Modulus, ASTM D790
- Flexural Modulus, ASTM D790
- Flexural Modulus, ASTM D790
- Flexural Modulus, ASTM D790
- Compressive Strength, ASTM D695
- Shear Strength, ASTM D732
- Izod Impact, Notched, ASTM D256
- Izod Impact, Notched, ASTM D256
- Izod Impact, Unnotched, ASTM D4812
- Izod Impact, Unnotched, ASTM D4812
- Charpy Impact Unnotched, ISO 179/1eU
- Volume Resistivity, ASTM D257
- Volume Resistivity, IEC 60093
- Surface Resistance, ASTM D257
- Surface Resistance, IEC 60093
- Dielectric Constant, ASTM D150
- Dielectric Constant, ASTM D150
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dielectric Strength, ASTM D149, Short Time
- Dissipation Factor, ASTM D150
- Dissipation Factor, ASTM D150
- Comparative Tracking Index, UL 746A
- CTE, linear, Parallel to Flow, ASTM E 228
- CTE, linear, Parallel to Flow, ASTM E 228
- CTE, linear, Parallel to Flow, ASTM E 228
- CTE, linear, Transverse to Flow, ASTM E 228
- CTE, linear, Transverse to Flow, ISO 11359-1/-2
- CTE, linear, Transverse to Flow, ASTM E 228
- CTE, linear, Transverse to Flow, ASTM E 228
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
- UL RTI, Electrical, UL 746B
- UL RTI, Electrical, UL 746B
- UL RTI, Electrical, UL 746B
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- Flammability, UL94, IEC 60695-11-10
- Flammability, UL94, IEC 60695-11-10
- Flammability, UL94, IEC 60695-11-10
- Flammability, UL94, UL94
- Flammability, UL94, UL94
- Flammability, UL94, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
|
| | |