MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Syensqo (Solvay Specialty Polymers) Amodel® AT-1116 HS PPA, 16% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: 16% glass fiber, impact modified, heat stabilized

Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stability, chemical resistance and ductility. This resin has a high heat deflection temperature and a high flexural modulus, with greater tensile elongation than untoughened glass reinforced PPA.

Typical applications include bearings, bearing retainers/cages, housings, chemical processing equipment components, motor frames, sporting equipment, lawn and garden equipment and components that require press-fit or snap-fit assembly.

- Black: AT-1116 HS BK 324
- Natural: AT-1116 HS NT

Markets/Uses: Automotive / Automotive E/E / Bobbins; Bus Bars; Connectors; Electric Vehicles; Engine Sensors; EV Recharger Connectors; Sensors; Wire Harness Connectors; Fuel Systems / Quick Connects

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Bobbins; Connectors; General Purpose; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement

Features: Chemical Resistant; Good Dimensional Stability; Heat Stabilized; High Heat Resistance; Impact Modified

Injection notes: Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ISO 1183, Method A
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength, ASTM D638
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180, Type 1, Notch A
  • Izod Impact, Unnotched (ISO), ISO 180, Type 1
  • Charpy Impact Unnotched, ISO 179, Type 1, Edgewise
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Dart Drop, Total Energy, ASTM D3763, Instrumented Dart Impact, Energy as Maximum Load
  • Dart Drop, Total Energy, ASTM D3763, Instrumented Dart Impact
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Melting Point, ASTM D3418, Peak
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  • Moisture Content, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.