MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Permabond 170 Cyanoacrylate, gap filling
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 will cure to a fixture strength in 15 seconds on most surfaces and strength development is rapid. The adhesive was designed specifically for the bonding of metal surfaces and provides excellent bond strength to steel, aluminum and most metal surface. The methyl cyanoacrylate will also adhere well to a wide variety of other materials including most plastics and rubbers. Permabond® 170 has been formulated to be less aggressive to sensitive plastic surfaces such as Styrofoam™, polycarbonate and ABS.

Features & Benefits:

  • Fast-setting
  • Ideal for bonding metals
  • Rapid development of high strength
  • Less aggressive to sensitive plastics

Information provided by Permabond.

Key Words: A-46060C Type I, Class 3
Vendors:
Available Properties
  • Specific Gravity, Uncured
  • Viscosity, Uncured
  • Storage Temperature
  • Hardness, Shore D, ISO 868
  • Adhesive Bond Strength, ISO 4587, Butyl rubber, Substrate Failure, Shear
  • Adhesive Bond Strength, ISO 4587, Nitrile rubber, Substrate Failure, Shear
  • Adhesive Bond Strength, ISO 4587, ABS, Substrate Failure, Shear
  • Adhesive Bond Strength, ISO 4587, Phenolic, Substrate Failure, Shear
  • Adhesive Bond Strength, ISO 4587, Acrylic, Shear
  • Adhesive Bond Strength, ISO 4587, Aluminum, Shear
  • Adhesive Bond Strength, ISO 4587, Stainless Steel, Shear
  • Adhesive Bond Strength, ISO 4587, Brass, Shear
  • Adhesive Bond Strength, ISO 4587, Steel, Shear
  • Impact, ASTM D950, kJ/m2 Adhesive Impact Strength
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Phenolic, handling time
  • Cure Time, Buna N Rubber, handling time
  • Cure Time, Steel, handling time
  • Cure Time, full strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.