MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Phillips 66 High Pressure Machine Oil ISO Grade 46
Categories: Fluid; Lubricant

Material Notes: Phillips 66® High Pressure Machine Oil is a high-quality, anti-wear lubricating oil developed for use in the fabrication of high-strength aluminum and aluminum alloy plates and sheets, such as those used in commercial and military aircraft, the aerospace industry, and in custom industrial applications. It is specially formulated to protect against distortion and provide excellent surface finish. High Pressure Machine Oil is formulated to provide excellent wear protection and surface finish during aluminum stretching operations. It has excellent antiwear properties and high load-carrying capacity to protect against distortion. It has excellent oxidation resistance at high temperatures to provide long service life and protect against deposit formation and staining. It has excellent water-separating properties to minimize the formation of emulsions, protects hydraulic system components against rust and corrosion, and is resistant to excessive foam buildup. It also has good low-temperature properties for cold start-ups. It is non-staining to aluminum, bronze, and brass. High Pressure Machine Oil meets the stringent minimum requirement for load-carrying capacity for hydraulic oils as measured by the Brugger Test.

Applications:

  • Fabrication of high-strength aluminum and aluminum alloy plates and sheets
  • Rolling and stretching of aluminum
  • Chain drives
Features/Benefits:
  • High load-carrying capacity to protect against metal distortion
  • Excellent surface finish
  • Non-staining
  • Excellent wear protection
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Good foam resistance
  • Good low-temperature performance

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D2272, RPVOT
  • ASTM Color, ASTM D1500
  • Total Acid Number, ASTM D974, [mg KOH/g]
  • Four Ball Wear, ASTM D4172, Scar Diameter
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.