Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. Glass-reinforced Vydyne resins provide higher hear distortion temperature, resistance to creep and better dimensional stability when compared with unreinforced PA66. These products have good chemical resistance to a broad range of chemicals including many aliphatic and aromatic hydrocarbons found in most solvents, gasoline, hydraulic fluids, greases and machine oils. Vydyne R543H NT resin has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption and part weight are key advantages of Vydyne glass-reinforced PA66 resins over aluminum and/or zinc die-cast parts. Vydyne R543H NT is formulated to minimize the oxidative and thermal degradation of the PA66 polymer when exposed to elevated temperatures for extended periods of time. Vydyne R543H NT provides improved retention of physical properties under exposure to long-term heat. The continuous operating use temperature is 275°F, with short-term peak temperatures as high as 475°F. Availability: - Asia Pacific
- Europe
- North America
Filler/Reinforcement:- Glass Fiber, 43% Filler by Weight
Additive: Features:- Gasoline Resistance
- Good Chemical Resistance
- Good Creep Resistance
- Good Dimensional Stability
- Good Impact Resistance
- Good Mold Release
- Grease Resistant
- Heat Stabilized
- High Flow
- High Rigidity
- High Strength
- High Tensile Strength
- Lubricated
- Oil Resistant
- Solvent Resistant
Uses:- Automotive Under the Hood
- Gears
- Housings
- Lawn and Garden Equipment
- Power/Other Tools
Appearance: Natural ColorForms: Pellets Processing Method: Injection Molding Information provided by Ascend Performance Materials. |