MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Arlon Electronic Materials 92ML High Performance Halogen-Free Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Thermally conductive, multilayerable laminate and prepreg circuit board material. Available in various resin content percentages.

Arlon 92ML ceramic filled thermally conductive multifunctional epoxy laminate and prepreg products provide thermal performance with increased thermal conductivity of 2 W/m-K for multilayer PWBs for applications requiring thermal management throughout the entire board volume.

  • Engineered for use with metal backing for producing Metal-Clad PCBs

Typical Applications:

  • High brightness LEDs
  • DC-DC power converters
  • Automotive electronics
  • Electronic designs with limited thermal management alternatives

Information provided by ARLON Electronic Materials.

Vendors:
Available Properties
  • Density, ASTM D792 Method A
  • Water Absorption, IPC TM-650 2.6.2.1
  • Tensile Strength, IPC TM-650 2.4.18.3
  • Flexural Strength, IPC TM-650 2.4.4
  • Peel Strength, IPC TM-650 2.4.8, To Copper (1 oz./35 micron); After Process Solutions
  • Peel Strength, IPC TM-650 2.4.8, To Copper (1 oz./35 micron); After Thermal Stress
  • Volume Resistivity, IPC TM-650 2.5.17.1, C96/35/90
  • Volume Resistivity, IPC TM-650 2.5.17.1, E24/125
  • Surface Resistance, IPC TM-650 2.5.17.1, C96/35/90
  • Surface Resistance, IPC TM-650 2.5.17.1, E24/125
  • Dielectric Constant, IPC TM-650 2.5.5.9
  • Dielectric Constant, IPC TM-650 2.5.5.3
  • Dielectric Strength, IPC TM-650 2.5.6.2
  • Dielectric Breakdown, IPC TM-650 2.5.6
  • Dissipation Factor, IPC TM-650 2.5.5.3
  • Arc Resistance, IPC TM-650 2.5.1
  • CTE, linear, IPC TM-650 2.4.41, x ,y direction
  • CTE, linear, Transverse to Flow, IPC TM-650 2.4.24, z (< Tg)
  • CTE, linear, Transverse to Flow, IPC TM-650 2.4.24, z (> Tg)
  • Thermal Conductivity, ASTM E1461, Z-axis
  • Thermal Conductivity, ASTM E1461, X/Y-axis
  • Glass Transition Temp, Tg, IPC TM-650 2.4.25, DSC
  • Glass Transition Temp, Tg, IPC TM-650 2.4.24, TMA
  • Decomposition Temperature, IPC TM-650 2.3.41, Onset
  • Decomposition Temperature, IPC TM-650 2.3.41, 5 percent
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.