MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Special Metals UDIMET® alloy 720 Nickel Base Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: UDIMET® alloy 720 is a nickel base alloy, solid solution strengthened with tungsten and molybdenum and precipitation-hardened with titanium and aluminum. The alloy combines high strength with metallurgical stability as demonstrated by excellent impact strength retention after long exposures at elevated temperatures. Good oxidation and corrosion resistance combined with high strength make the alloy useful in gas turbine blade and disc applications.

Information Provided by Special Metals Corporation

Key Words: EMS 55477; EMS 73105; MSRR 7252; C50TF105; MTS 5013
Vendors:
Available Properties
  • Density
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • CTE, linear
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Molybdenum, Mo
  • Nickel, Ni, Balance
  • Titanium, Ti
  • Tungsten, W
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Special Metals (includes the former Inco Alloys International Inc.)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.