MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP30AO Thermally Conductive Low Viscosity Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Thermally conductive
  • Electrically insulative
  • High compressive strength
  • Low thermal expansion coefficient
  • Low mixed viscosity with excellent flowability
  • Superior dimensional stability
Product Description: Master Bond EP30AO is a two component epoxy resin system for high performance potting, bonding, sealing and coating, formulated to cure at room temperature or more rapidly at elevated temperatures with a ten to one mix ratio by weight. It has an attractive balance of performance properties including high thermal conductivity, excellent electrical insulation characteristics and superior dimensional stability, as well as outstanding physical strength properties. EP30AO has a low viscosity with excellent flow characteristics making it ideal as a thermally conductive, potting epoxy. EP30AO is also a superb adhesive/sealant forming durable, rigid bonds that are resistant to thermal cycling and chemicals including water, oils and most solvents, over the wide temperature range of -60°F to +250°F. The thermal expansion coefficient is desirably low. Color of Part A is off white, Part B is clear. EP30AO is widely used in the electronic, electrical, computer, metalworking, appliance, automotive and chemical industries where electrical insulation an environmental protection are required and heat transfer must be maintained.

Product Advantages:

  • Easy application: adhesive spreads or pours evenly and smoothly
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required
  • High bond strength to a wide variety of substrates; excellent adhesion properties
  • Good physical strength characteristics
  • Outstanding resistance to a wide range of chemicals

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.