Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties, excellent surface quality and excellent flammability rating. - Black: Kalix® 9945 BK000 HFFRKey Attributes: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Paintable; Platable Applications: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts Typical values shown tested on Dry as Molded samples. Standard Packaging and Labeling: - Kalix® resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the product number, the color, the lot number, and the net weight. Injection Notes: Storage: - Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding. Drying: - Kalix® compounds are supplied in sealed bags. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts. - Drying temperatures of up to 100°C may be used for dark colored resin (such as black) to achieve shorter drying times, if necessary. For lighter colored resin, 80°C drying temperature is recommended to minimize the risk of oxidative discoloring. - Use of a desiccant dryer with -40°C dew point is strongly suggested to ensure Kalix® material has reached optimum moisture content before processing. Injection Molding: - Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled. Information provided by Solvay Specialty Polymers. |