MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Hexcel® HexPly® M76/IM7 Curing Epoxy Matrix/Unidirectional Tape
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by Hexcel Corporation.

Vendors:
Available Properties
  • Tensile Strength, pr EN 2561 type B, M76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm
  • Tensile Strength, pr EN 2561 type B, M76/42%/G793/C, 5HS high strength fiber 280 gsm
  • Tensile Strength, pr EN 2561 type B, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Tensile Strength, 90°
  • Tensile Strength, Onset, Edge Delamination
  • Tensile Strength, Ultimate, Edge Delamination
  • Tensile Strength, 0°
  • Tensile Strength, 0°
  • Elongation at Break, 90°
  • Elongation at Break, 0°
  • Elongation at Break, 0°
  • Tensile Modulus, pr EN 2561 type B, M76/42%/G793/C, 5HS high strength fiber 280 gsm
  • Tensile Modulus, pr EN 2561 type B, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Tensile Modulus, pr EN 2561 type B, M76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm
  • Tensile Modulus, Wet, IPS Properties (±45° tension)
  • Tensile Modulus, Wet, IPS Properties (±45° tension)
  • Tensile Modulus, Wet, IPS Properties (±45° tension)
  • Tensile Modulus, IPS Properties (±45 tension)
  • Tensile Modulus, 90°
  • Tensile Modulus, 0°
  • Tensile Modulus, 0°
  • Flexural Strength, 0°, Wet
  • Flexural Strength, 0°, Dry
  • Flexural Strength, 0°
  • Flexural Modulus, 0°, Wet
  • Flexural Modulus, 0°, Dry
  • Flexural Modulus, 0°
  • Compressive Strength, After Impact (25/50/25 orientation), 1500 in-lb/in. impact level
  • Compressive Strength, Open Hole (25/50/25 orientation), wet
  • Compressive Strength, Open Hole (25/50/25 orientation)
  • Compressive Strength, pr EN 2850 type A, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Compressive Strength, pr EN 2850 type A, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
  • Compressive Strength, pr EN 2850 type A, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
  • Compressive Strength, pr EN 2850 type A, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Compressive Strength, 0°, Wet
  • Compressive Strength, 0°, Dry
  • Compressive Strength, 0°
  • Compressive Modulus, pr EN 2850 type A, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
  • Compressive Modulus, pr EN 2850 type A, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Compressive Modulus, pr EN 2850 type A, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
  • Compressive Modulus, pr EN 2850 type A, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Shear Strength, Interlaminar, M76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm
  • Shear Strength, Interlaminar, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Shear Strength, Interlaminar, M76/42%/G793/C, 5HS high strength fiber 280 gsm
  • Shear Strength, Interlaminar, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
  • Shear Strength, Interlaminar, M76/42%/G1087/C, 5HS M46J high modulus fiber 275 gsm
  • Shear Strength, Interlaminar, 0°, Wet
  • Shear Strength, Interlaminar, M76/42%/G1094/C, 5HS intermediate modulus fiber 290 gsm
  • Shear Strength, Interlaminar, M76/42%/G793/C, 5HS high strength fiber 280 gsm
  • Shear Strength, Interlaminar, M76/42%/G1089/C, Twill 2x2 intermediate modulus fiber 200 gsm
  • Shear Strength, Interlaminar, 0°, Dry
  • Shear Strength, Interlaminar, 0°
  • Tensile Impact, Interlaminar Fracture, (DCB)
  • Tensile Impact, Interlaminar Fracture, (ENF)
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.