MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Zortrax Zortrax Resin Basic White, Ivory, Grey
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Zortrax Resin Basic is a versatile light-cured resin that’s been developed to work with the Zortrax Inkspire. This material is best suited to the needs of users from various fields, whose job involves creating intricate and highly detailed models. Zortrax Resin gives a possibility to print parts of high quality and provides precision unmatched by traditional 3D printing technologies. Thanks to the impeccable accuracy, Zortrax Resin becomes the best choice for creating prototypes and concept models in engineering, as well as for creative applications, such as figurines and gadgets.

Information provided by Zortrax

Vendors:
Available Properties
  • Density
  • Viscosity
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Flexural Strength
  • Flexural Modulus
  • Izod Impact, Notched
  • Glass Transition Temp, Tg
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.