MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Wacker Vinnapas® 192 Polymer Dispersion
Categories: Polymer

Material Notes: Product description: VINNAPAS® 192 (CGN) is a self crosslinking, plasticizer-free, aqueous polymer dispersion produced from the monomers vinyl acetate and ethylene for the Nonwovens market.

Application: General VINNAPAS® 192 (CGN) offers a unique balance of high dry and wet strength, excellent absorbent properties, and imparts good handfeel. The dispersion is stabilized with an APE-free surfactant and has a low formaldehyde content of less than 100 ppm. Special VINNAPAS® 192 (CGN) can be applied by a number of different application methods including saturation, spraying, foaming and print bonding. VINNAPAS® 192 (CGN) performs well on various fiber types including cellulose, rayon, glass and polyester. This dispersion is especially suited for use in feminine hygiene and related absorbent products, and premoistened wipes. Temperatures above 150°C are necessary to achieve proper crosslinking.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, DIN EN ISO 2881-3
  • Solids Content, DIN EN ISO 3251
  • Particle Size
  • pH, DIN/ISO 976
  • Viscosity, DIN EN ISO 25555, dynamic
  • Tensile Strength at Break, DIN EN ISO 527, part 1-3, crosslinked
  • Elongation at Break, DIN EN ISO 527, part 1-3, crosslinked
  • Glass Transition Temp, Tg
  • Transmission, Visible, "Clear" but manufacturer does not quantify.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.