Homopolymer
Features:
Additive Packages:
Applications:
United States: NOVAPOL PF-0118 Series resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.
NOVA Chemicals polyethylene resins are biologically and chemically inert.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic