MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Henkel Loctite® Stycast® 2850 MT CAT 11 Two-Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 2850 MT CAT 11 provides the following product characteristics:
  • High thermal conductivity
  • Low CTE
  • Long pot life
  • Excellent chemical resistance
  • Good physical and chemical properties at elevated temperatures

Cure: Heat cure

Application: Encapsulation

Loctite Stycast 2850 MT CAT 11 is recommended for encapsulation of components that require heat dissipation and thermal shock properties. It is also recommended for use in high voltage applications where surface arching or tracking is a concern. Loctite Stycast 2850 MT CAT 11 has a slightly grainy consistency due to the filler size.

Loctite Stycast 2850 MT can be used with a variety of catalysts.

Information provided by Henkel.

Vendors:
Available Properties
  • Density, Part A, Loctite Stycast 2850MT
  • Density, Mixed
  • Water Absorption
  • Viscosity, Part B, Loctite CAT 11
  • Brookfield Viscosity, Mixed
  • Brookfield Viscosity, 2.5 rpm, #6, Part A, Loctite Stycast 2850MT
  • Linear Mold Shrinkage
  • Outgassing - Total Mass Loss, CVCM, NASA Method, Sample cured 24 hours @ 74ºC
  • Outgassing - Total Mass Loss, TML, NASA Method, Sample cured 24 hours @ 74ºC
  • Hardness, Shore D
  • Flexural Strength
  • Compressive Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, Option 3. Post cure of 2 to 4 hours at the highest expected use temperature is recommended.
  • Cure Time, Option 2. Post cure of 2 to 4 hours at the highest expected use temperature is recommended.
  • Cure Time, Option 1. Post cure 2 to 4 hours at the highest expected use temperature is recommended.
  • Working Life, 100 g mass
  • Shelf Life, Part A, Loctite Stycast 2850MT
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.