MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Mobilgrease 27
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 and No. 2 grease. It offers outstanding performance over a wide temperature range. The thickener system provides excellent structural stability and resistance to water wash. The properties of the base oil, combined with selected additives, provide outstanding protection against rust, corrosion, wear and high temperature degradation. The synthetic base oil allows for low-temperature mobility/pumpability and very low starting and running torque values.

Mobilgrease 27 is a true multipurpose aviation grease intended for use in highly loaded gears and actuators as well as instruments, high speed bearings (though not recommended for wheel bearings), and general airframe lubrication over temperatures from –100ºF to 250ºF. Mobilgrease 27 is also an excellent choice for applications where a smooth, low noise, wide temperature range lubricating grease is required, such as in miniature precision bearings. Mobilgrease 27 contains a synthetic ester and should not be used in contact with incompatible seal materials. It may soften natural rubber, neoprene, certain electrical insulation materials and paints. Mobilgrease 27 meets the requirements and is approved against U.S. Military Specification MIL-PRF-23827, Grease, Aircraft and Instrument, Gear and Actuator Screw, Type I (Grease thickened with metallic soap). It is listed in the QPL-23827 Qualified Products List. In addition, Mobilgrease 27 may be used in all applications where MIL-G-3278, MIL-G-7118, MIL-G-7421, MIL-G-15793 and MIL-G-23827 are specified, subject to approval by the aircraft manufacturer. It is a NATO Code Number G-354 grease.

Key Words: NLGI Grade 1.5
Vendors:
Available Properties
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Oxidative Stability, ASTM D942, Pressure Drop of less than 70 kPa @ 99°C
  • Oxidative Stability, ASTM D942, Pressure Drop of less than 105 kPa at 99°C
  • Evaporation Loss, ASTM D2595, 22 hrs @ 100°C
  • Storage Temperature, FTM 3467, 6 months time
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2596
  • Penetration, ASTM D217, Unworked, 25°C
  • Penetration, ASTM D445, 60 Stroke Worked, 25°C
  • Penetration, FTM 313, Extended Worked Penetration Stability, 100000 Strokes, mm/10
  • Oil Separation, ASTM D6184, 30 hrs @ 100°C
  • Dropping Point, ASTM D2265
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.