ASTM A36 Steel, bar
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Steel for general structural purposes including bridges and buildings.

Key Words: UNS K02600
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 400 - 550 MPa58000 - 79800 psi
Tensile Strength, Yield 250 MPa36300 psi
Elongation at Break 20 %20 %in 200 mm
 23 %23 %In 50 mm.
Modulus of Elasticity 200 GPa29000 ksi
Compressive Yield Strength 152 MPa22000 psiAllowable compressive strength
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.260.26
Shear Modulus 79.3 GPa11500 ksi
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.29 %0.29 %
Copper, Cu >= 0.20 %>= 0.20 %only if copper steel is specified
Iron, Fe 98 %98 %
Manganese, Mn 0.80 - 1.2 %0.80 - 1.2 %
Phosphorus, P 0.040 %0.040 %
Silicon, Si 0.15 - 0.40 %0.15 - 0.40 %
Sulfur, S 0.050 %0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.