Medium setting: general purpose adhesive designed to bond a wide variety of similar or dissimilar materials. The product is a versatile adhesive offering good climatic, thermal and impact resistance. Its elasticity makes it ideal for bonding dissimilar materials. Handling strength in 5 to 10 seconds. RP 5 has a viscosity of 5 cps and is capable of filling gaps up to .002Information provided by Adhesive Systems, Inc. |