MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® AVS4BC1 BK0886 PA66-GF35
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Vydyne AVS4BC1 BK0886 is part of Ascend's Anti-Vibration System portfolio. AVS4BC1 BK0886 is a 35% glass filled PA66 specialty compound that is specifically designed to provide a good balance of energy absorption and mechanical stiffness for critical NVH components.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDAM; ISO 1183
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.4 %
@Temperature 23.0 °C
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 151 MPa50% RH; ISO 527-2
 197 MPaDAM; ISO 527-2
Elongation at Break 2.7 %DAM; ISO 527-2
 3.0 %50% RH; ISO 527-2
Tensile Modulus 9900 MPa50% RH; ISO 527-2
 11500 MPaDAM; ISO 527-2
Flexural Strength 193 MPa50% RH; ISO 178
 287 MPaDAM; ISO 178
Flexural Modulus 8700 MPa50% RH; ISO 178
 11100 MPaDAM; ISO 178
Poissons Ratio 0.34ISO 527-2
Izod Impact, Notched (ISO) 8.90 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 8.90 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 9.50 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 59.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 64.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 65.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 65.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 82.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 8.60 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 8.70 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 26.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 257 °CUnannealed; 50% RH; ISO 75-2/B
 258 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 236 °CUnannealed; 50% RH; ISO 75-2/A
 244 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature >= 280 °CInjection
 <= 310 °CInjection
Middle Barrel Temperature >= 280 °CInjection
 <= 310 °CInjection
Front Barrel Temperature >= 280 °CInjection
 <= 310 °CInjection
Nozzle Temperature >= 280 °CInjection
 <= 310 °CInjection
Melt Temperature >= 285 °CInjection
 <= 305 °CInjection
Mold Temperature >= 65.0 °CInjection
 <= 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.15 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA0100A5438
 ASTM, D6779 PA0100A5438
 ISO, 1043 PA66 GF35
AppearanceBlack
FeaturesBalanced Stiffness/Toughness
 Fatigue Resistant
 Good Dimensional Stability
 Good Stiffness
 Good Tensile Strength
 Heat Stabilized
 Lubricated
FormsPellets
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8494 / 318011

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.