Elastic, moisture curing, one component adhesive suitable as bedding compound in the marine and boat industry- Bedding compound for teak decks
- Overpaintable after curing
- Good resistance to humidity and weathering extensive bonding of teak decking
- Resistant to temperature from -40°C to +90°C (for short intervals up to +120°C)
- Meets the requirements of the International Maritime OrganizationInformation provided by H.B. Fuller Company
|