MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ 2312EPR PEI (Europe)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 30% Glass Fiber

Material Notes: 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Density 1.48 g/ccISO 1183
Moisture Absorption 0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.90 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmon Tensile Bar; SABIC method
 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 13.7 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 14 g/10 min
@Load 5.00 kg,
Temperature 360 °C
MVR, cm^3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527
 94.0 MPaType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 80.0 MPa5 mm/min; ISO 527
 94.0 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 2.0 %5 mm/min; ISO 527
 2.0 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 2.0 %5 mm/min; ISO 527
 2.0 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 145 MPa2 mm/min; ISO 178
 156 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5500 MPa2 mm/min; ISO 178
 5580 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 39.0 J/mASTM D256
Izod Impact, Unnotched 330 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1U
 25.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 25.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 25.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 15.0 JASTM D3763
Tangent Modulus 5300 MPa1 mm/min; ISO 527
 6480 MPa5 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 secUL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
 32.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 35.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
 35.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.320 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 204 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 204 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 206 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 192 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 199 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 202 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 211 °CRate B/50; ISO 306
 213 °CRate B/120; ISO 306
 216 °CRate B/50; ASTM D1525
Flammability, UL94 V-0
@Thickness 0.400 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 1 330 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °C
Mold Temperature 135 - 165 °C
Drying Temperature 150 °C
Dry Time 4.00 - 6.00 hour
 24.0 hourCumulative
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
THERMALPassesIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI22675 / 215811

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.