Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.25 g/cc | 1.25 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 79 | 79 |
| 55 @Temperature 150 °C, Time 252000 sec | 55 @Temperature 302 °F, Time 70.0 hour |
| 74 @Temperature 225 °C, Time 252000 sec | 74 @Temperature 437 °F, Time 70.0 hour |
| 74 @Temperature 150 °C, Time 252000 sec | 74 @Temperature 302 °F, Time 70.0 hour |
| 76 @Temperature 200 °C, Time 252000 sec | 76 @Temperature 392 °F, Time 70.0 hour |
| 78 @Temperature 100 °C, Time 252000 sec | 78 @Temperature 212 °F, Time 70.0 hour |
Tensile Strength | 9.115 MPa | 1322 psi |
| 6.508 MPa @Temperature 225 °C, Time 252000 sec | 943.9 psi @Temperature 437 °F, Time 70.0 hour |
| 8.1034 MPa @Temperature 150 °C, Time 252000 sec | 1175.3 psi @Temperature 302 °F, Time 70.0 hour |
| 8.5405 MPa @Temperature 200 °C, Time 252000 sec | 1238.7 psi @Temperature 392 °F, Time 70.0 hour |
Elongation, Ultimate | 420 % | 420 % |
| 215.5 % @Temperature 225 °C, Time 252000 sec | 215.5 % @Temperature 437 °F, Time 70.0 hour |
| 325 % @Temperature 200 °C, Time 252000 sec | 325 % @Temperature 392 °F, Time 70.0 hour |
| 330.5 % @Temperature 150 °C, Time 252000 sec | 330.5 % @Temperature 302 °F, Time 70.0 hour |
100% Modulus | 3.05 MPa | 443 psi |
Tear Strength | 24.5 kN/m | 140 pli |
| 25.2 kN/m | 144 pli |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | <= -65.0 °C | <= -85.0 °F |
Shrinkage | 0.30 % @Temperature 100 °C, Time 252000 sec | 0.30 % @Temperature 212 °F, Time 70.0 hour |
| 0.30 % @Temperature 100 °C, Time 252000 sec | 0.30 % @Temperature 212 °F, Time 70.0 hour |
| 2.7 % @Temperature 150 °C, Time 252000 sec | 2.7 % @Temperature 302 °F, Time 70.0 hour |
| 4.3 % @Temperature 150 °C, Time 252000 sec | 4.3 % @Temperature 302 °F, Time 70.0 hour |
| 29.4 % @Temperature 150 °C, Time 252000 sec | 29.4 % @Temperature 302 °F, Time 70.0 hour |
| 40.6 % @Temperature 150 °C, Time 252000 sec | 40.6 % @Temperature 302 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Grey |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding