MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior ForTii® Ace JTX8 PPA-GF30 PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide with halogen-free and halogen containing flame retardant grades for demanding applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

Ace JTX8 is the only polyamide grade in the world that secures, in all product designs, the JEDEC MSL 1 rating at all thicknesses. Ace JTX8 has the highest Tg available in polyamides (160°C) to satisfy various industry requirements like chemical resistance and high temperature thermal ageing. Ace JTX8 has robust processing performance and allows 100% regrinding with high mechanical properties retention. Processing: Injection molding. 30% glass reinforced.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccDry; ISO 1183
Moisture Absorption 2.00 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0043 cm/cmDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cmDry; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPa
@Temperature 200 °C
ISO 527-1/-2
 100 MPa
@Temperature 160 °C
ISO 527-1/-2
 120 MPa
@Temperature 80.0 °C
Cond; ISO 527-1/-2
 150 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 170 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 180 MPa
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 190 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 200 MPa
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 210 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 240 MPa
@Temperature -40.0 °C
Dry; ISO 527-1/-2
Elongation at Break 2.5 %
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 2.6 %
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 2.7 %
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 2.7 %
@Temperature 100 °C
Dry; ISO 527-1/-2
 2.8 %
@Temperature -40.0 °C
Dry; ISO 527-1/-2
 2.8 %
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 3.0 %
@Temperature 80.0 °C
Cond; ISO 527-1/-2
 3.0 %
@Temperature 120 °C
Dry; ISO 527-1/-2
 5.0 %
@Temperature 160 °C
Dry; ISO 527-1/-2
 6.0 %
@Temperature 200 °C
Dry; ISO 527-1/-2
Tensile Modulus 4000 MPa
@Temperature 200 °C
Dry; ISO 527-1/-2
 6000 MPa
@Temperature 160 °C
Dry; ISO 527-1/-2
 9500 MPa
@Temperature 80.0 °C
Cond; ISO 527-1/-2
 9500 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 10200 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 10300 MPa
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 10500 MPa
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 11000 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 11000 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 11700 MPa
@Temperature -40.0 °C
Dry; ISO 527-1/-2
Flexural Strength 275 MPaCond; ISO 178
 300 MPaDry; ISO 178
Flexural Modulus 3900 MPa
@Temperature 200 °C
ISO 178
 5700 MPa
@Temperature 160 °C
ISO 178
 9500 MPa
@Temperature 120 °C
ISO 178
 10500 MPa
@Temperature 23.0 °C
Dry; ISO 178
 10500 MPa
@Temperature 23.0 °C
Cond; ISO 178
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -30.0 °C
Cond; ISO 179/1eU
 60.0 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eU
 65.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
Cond; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Constant 3.83
@Frequency 1e+10 Hz
Dry; IEC 60250
 3.88
@Frequency 1e+9 Hz
Cond; IEC 60250
 3.92
@Frequency 1e+9 Hz
Dry; IEC 60250
Dielectric Strength 40.0 kV/mmCond; IEC 60243-1
 45.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VDry; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 18.0 µm/m-°Cdry; ISO 11359-1/-2
Melting Point 340 °C10°C/min. Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 174 °CThermal Index; 5000 hrs.; IEC 60216/ISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 320 °CDry; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 3.00 mm
Dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7906 / 291342

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.