Base Polymer: Polypropylene Homopolymer Filler/Additive System: 30% glass fiber Special Features: Chemically coupled, high heat stabilized, high stiffness, high toughness Market Segment: Automotive Typical Applications: Various Information provided by Albis Plastics |