Riblene FM 50 F is a LDPE suitable for blown film extrusion. Riblene FM 50 F is characterized by optimum optical properties and rigidity. Films manufactured by Riblene FM 50 F are easily heat shrinkable. Application: Riblene FM 50 F is recommended for automatic packaging where low gauge films having a certain rigidity and gloss are required (hygienic packaging). Property values reported for film extruded with BUR 1:3, thickness 70 µm. Actual properties are typical and may vary depending upon operating conditions and additive package. Information provided by Versalis. |