Compound 3606 is a 60 durometer medium high nitrile Buna N elastomer. It exhibits good physical properties. It exhibits good resistance to oils and greases. It will also remain non brittle at low temperatures. This compound is ADCF. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 620 B14 B34 EO14 EO34; 2 BG 620 B14 B34 EA14 EF11 EF21 EO14 EO34 F17; 3 BG 620 B14 EO14; 4 BG 620 A14 B14; 5 BG 620 A14 B14 B34 EO14 EO34; 4 BK 620 A24 B14 B34 EF11 EO14 Information provided by Pressure Seals Inc. |