MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Danquinsa DANADD® S-01 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® S-01 is a modified additive to improve the adhesion of the rubber in combination with Polyurethane adhesives.

Application: DANADD® S-01 is used only as an additive for Polyurethane adhesives, for the adhesion of roughen rubber materials. DANADD® S-01 is added directly in the solvent mixture and together with the PEARLSTICK®- PUR- adhesives dissolved. We recommend a addition of 0,3% up to 0,5 %, referring to the processed adhesive solvent. With DANADD® S-01 modified adhesive solvents should not exceed a storage time of 8 month. Otherwise there must be a loss of viscosity calculated if the storage time is overdue.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³DIN 51.757
Solids Content 100 %100 %DIN 53.189
Storage Temperature 0.000 - 40.0 °C32.0 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °FKOFLER
Softening Point 130 °C266 °FKOFLER
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectwhite even powder
Dosage0.3-0.5%
TypeModified di carboxylic acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ015 / 294435

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.