MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Virantage® VW-10300SFP providing three particle sizes to meet formulators' specific needs. Their inherent toughness imparts damage tolerance to thermoset composites. Virantage® PESU polymers also offer superior thermal and hydrolytic stability that deliver best-in-class hot-wet performance.

These amorphous thermoplastics may be used to toughen a variety of advanced thermoset composites used to produce high-performance aerospace components. Virantage® PESU tougheners have been used successfully in a variety of thermosetting resin systems including epoxies, phenolics and BMIs.

Key Attributes: Amorphous; Good Thermal Stability; Good Toughness; High Heat Resistance; Hydrolytically Stable; Medium Molecular Weight; Medium-high Viscosity

Applications: Aerospace Applications

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 800 cPSolution Viscosity; ASTM D445
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 220 °CASTM E1356
 
Descriptive Properties
Availability (as of March 2019)Africa & Middle East; Asia Pacific; Europe; Latin America; North America
FormsPowder
ProcessingCompounding

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y5484 / 238865

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.