Semi-flexible polyurethane elastomer Key Properties: - Excellent physical properties after RT cure
- Free of mercury, MOCA or TDI
Applications: - For hand-batch or vacuum assisted processing
Cure 1: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |