MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Vulcan® 6-LP Carbon Black
Categories: Carbon; Carbon Black

Material Notes: Product Description: Carbon Blacks are the most utilized fillers in the Rubber Industry. Based on its cost and performance, no other filler can match the properties of carbon black. Used for nearly 100 years, carbon blacks have been reinforcing rubber compounds both physically and chemically. Cabot Corporation has been producing carbon blacks for nearly 120 years and is now the world leader in the manufacturing of this essential ingredient. As part of Cabot’s ongoing commitment to address changing marketplace needs and deliver solutions to meet our customers’ future product design and processing challenges, Cabot has developed a series of low polycyclic aromatic hydrocarbons (PAH) carbon blacks, identified by the suffix “LP.” The Cabot LP carbon black series is manufactured via a special process resulting in a controlled, very low level of PAH. Vulcan 6-LP carbon black is a member of the Cabot LP carbon black series. It is a pelletized reinforcing carbon black and is characterized by a controlled, very low PAH content.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 35 Mesh<10 ppm, Residue; ASTM D1514
 325 Mesh<500 ppm, Residue; ASTM D1514
Ash <= 1.0 %ASTM D1506
 
Descriptive Properties
Absorption114 ml/100gDBP, ASTM D2414
 121 g/KgIodine Absorption Number, ASTM D1510
Heat Loss0.01ASTM D1509

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH040 / 314958

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.