MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akrochem ELAZTOBOND A250 Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: ELAZTOBOND A250 Resin is a modified phenol formaldehyde resin developed to replace resorcinol resins. In combination with a methylene donor such as hexamethylenetetramine (AKROFORM® HMT-80/EPR/P) or hexamethoxymethylmelamine (AKROSPERSE® HMMM-50/EPR/S), ELAZTOBOND A250 Resin functions as an adhesion promoter additive to the rubber compound. Typical applications for this type of adhesive system include bonding rubber to rubber, fabric or steel cord.

Applications: ELAZTOBOND A250 Resin is utilized as an adhesion promoter, resorcinol replacement in RFS (Resorcinol-Formaldehyde-Silica) bonding systems, also known as HRH systems. The RFS system has been a proven adhesion mechanism for many years bonding natural and synthetic rubbers to treated and untreated fabrics, metals and rubbers. This adhesion system uses ELAZTOBOND A250 in combination with a methylene donor, typically hexamethylenetetramine (hexa) and silica. The typical loadings of ELAZTOBOND A250, hexa and silica are 2.5, 1.6 and 10 phr, respectively. Many compounders will adjust these loadings to obtain optimal bonding properties for their application. The ELAZTOBOND A250, hexa, and silica loadings typically fall within the following ranges: 2-4, 1-4 and 10-25 phr, respectively. This thermoplastic resin has replaced straight resorcinol in many applications due to improved dispersibility, adhesion performance and health concerns. ELAZTOBOND A250 is especially important in polychloroprene (CR) fabric adhesion, since normal resorcinol can scorch CR. Excellent methylene donor in CR is hexamethoxymethylmelamine (HMMM). It is very important that the ELAZTOBOND A250 is well dispersed in the first pass. The methylene donor is added during the second pass of the mixing process. Filler and accelerator adjustments may be necessary to maintain hardness and cure rate.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/cc
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 100 - 110 °C212 - 230 °F
 
Descriptive Properties
AppearanceFlake

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH395 / 315313

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.