MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECACOMP PP HTE PW black 1014974 Polypropylene, Graphite Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
  • high electrical conductivity
  • high thermal conductivity
  • very good chemical resistance
  • for hot compression molding
Target Industries:
  • bipolar plates for fuel cells
  • separator plates for redox-flow batteries

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.96 g/cc
Water Absorption at Saturation <= 0.10 %50 % relative humidity up to saturation; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 37.0 MPaDIN EN ISO 178
Flexural Modulus 12300 MPaDIN EN ISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.59 ohm-cmDIN EN ISO 3915
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 20.0 W/m-Kthrough-plane; ISO 22007-4:2008
 66.0 W/m-Kin-plane; ISO 22007-4:2008
Melting Point 165 °C
Maximum Service Temperature, Air 90.0 °Clong term
 130 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 148 °CISO-R 75 Method A
Minimum Service Temperature, Air -30.0 °C
Glass Transition Temp, Tg 0.000 °C
 
Descriptive Properties
Colorblack
Specific electrical conductivity168 S/cmDIN EN ISO 3915

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO9114 / 319042

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.