MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo Celanex® 2500-6FC PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Product Description: Celanex 2500-6FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processability for use in food contact applications. Celanex 2500-6FC is a medium to high flow material that contains a lubricant and nucleant additive package.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Additive: Mold Release

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Melt Density 1.11 g/cc0.0401 lb/in³Fill Analysis, Melt
Water Absorption 0.20 %0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.45 %0.45 %ISO 62
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.018 - 0.023 cm/cm0.018 - 0.023 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.018 - 0.021 cm/cm0.018 - 0.021 in/inISO 294-4
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 250 °C
40 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527-2/50
Tensile Strength, Yield 62.0 MPa8990 psiISO 527-2/50
Elongation at Break 15 %15 %Nominal; ISO 527-2/50
Elongation at Yield 4.0 %4.0 %ISO 527-2/50
Tensile Modulus 2.70 GPa392 ksiISO 527-1
Charpy Impact Unnotched  13.0 J/cm²
@Temperature -30.0 °C
62.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 13.4 J/cm²
@Temperature 22.8 °C
64.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.441 J/cm²
@Temperature -30.0 °C
2.10 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.504 J/cm²
@Temperature 22.8 °C
2.40 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.0 µin/in-°FISO 11359-2
Specific Heat Capacity 1.92 J/g-°C0.459 BTU/lb-°FFill Analysis, Melt
Thermal Conductivity 0.133 W/m-K0.920 BTU-in/hr-ft²-°FFill Analysis, Melt
Melting Point 225 °C437 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FUnannealed; ISO 75-2/A
Vicat Softening Point 190 °C374 °FISO 306/B50
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °FHopper
 250 - 260 °C482 - 500 °FHot Runner
Feed Temperature 190 - 200 °C374 - 392 °FInjection
Rear Barrel Temperature 240 - 250 °C464 - 482 °F
Middle Barrel Temperature 240 - 250 °C464 - 482 °F
Front Barrel Temperature 245 - 255 °C473 - 491 °F
Nozzle Temperature 250 - 260 °C482 - 500 °F
Zone 4 245 - 255 °C473 - 491 °FInjection
Melt Temperature 250 - 260 °C482 - 500 °F
Mold Temperature 75.0 - 85.0 °C167 - 185 °F
Ejection Temperature 219 °C426 °FFill Analysis
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6189 / 310882

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.