MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Persian Gulf Polymer PP-EP440G Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: EP440G is a nucleated heterophasic copolymer especially developed for extrusion applications. ?EP440G? exhibits high stiffness, very high impact properties at room and sub-zero temperatures, good dimensional stability and excellent creep and deforming resistance. The main applications of EP440G? are thermoforming, corrugated board and extrusion blow molding. Processing Method: Thermoforming, Extrusion blow molding. Features: Very high impact resistance, High stiffness, Good dimensional stability. Typical Applications: Crates, Panels & Profiles, Corrugated Sheet, Conduit pipes and fittings for electrical distribution and cable protection, Blow molded bottles and containers.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 1.3 g/10 min1.3 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiISO 527-1,-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 8.0 %8.0 %ISO 527-1,-2
Flexural Modulus 1.45 GPa210 ksiISO 527-1,-2
Charpy Impact, Notched  0.900 J/cm²
@Temperature 0.000 °C
4.28 ft-lb/in²
@Temperature 32.0 °F
Notch A; ISO 179
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Notch A; ISO 179
 
Optical PropertiesMetricEnglishComments
Gloss 65 %65 %60°; DIN 67350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI979 / 250383

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.