MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical XY-9335B Compound antioxidant
Categories: Other Engineering Material

Material Notes: The product of antioxidant complex YZ-9335B is compounded and granulated by a special process with the main antioxidant YZ-1010, auxiliary antioxidant YZ-168, highly active auxiliary antioxidant YZ-626 and the stabilizing agent in certain proportion. The product, a new generation of high-temperature antioxidant, is of good stability, showing the performance of excellent processing stability and color protection for resins such as polyolefin (PE, PP), PBT, and PET, which are processed in high temperature and need high color-protection. The product works specially well for polypropylene fiber spinning and the repeated high-temperature extrusion processing of plastic products. The product is particularly used in polypropylene brand T30S.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 2.0 %
 
Descriptive Properties
Appearancecolorless or yellowish oily liquid
Content<2.0%Alkyl phenol
Grain diameter1-3 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX026 / 317873

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.