MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plaskolite Optix® CP-927HF PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Availability: Europe; North America

Features: Chemical Resistant; Electrically Insulating; Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Weather Resistance; High Clarity; High Flow; Low Odor; Low to No Taste; Machinable

Appearance: Colors Available

Form: Pellets

Processing Method: Injection Molding

Information provided by Plaskolite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 11 g/10 min
@Load 3.80 kg,
Temperature 230 °C
11 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5353ASTM D785
Tensile Strength at Break 50.3 MPa7300 psiASTM D638
Elongation at Break 18 %18 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
Izod Impact, Unnotched 6.94 J/cm13.0 ft-lb/inASTM D4812
Gardner Impact 2.82 J2.08 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 75.6 µm/m-°C
@Temperature -30.0 - 30.0 °C
42.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C172 °FUnannealed; ASTM D648
Vicat Softening Point 93.3 °C200 °FASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Haze 2.0 %2.0 %ASTM D1003
Transmission, Visible 91 %91 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 249 °C400 - 480 °F
Middle Barrel Temperature 210 - 254 °C410 - 490 °F
Front Barrel Temperature 216 - 260 °C420 - 500 °F
Nozzle Temperature 210 - 260 °C410 - 500 °F
Melt Temperature 210 - 249 °C410 - 480 °F
Mold Temperature 48.9 - 79.4 °C120 - 175 °F
Drying Temperature 65.6 - 73.9 °C150 - 165 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLASKO837 / 311530

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.